Before approving the draft of a textured enclosure, the CAD model and finish specification must agree on the ejection direction, where texture starts and stops, which faces are cosmetic, and how sample parts will be judged. This checklist walks through the decisions that product engineers and tooling buyers should mark on the model and finish spec so that the mold maker, texture supplier and molder work from the same intent. It focuses on qualitative review steps rather than universal angle rules, because draft depends on material, texture depth, part geometry and ejection depth.

Start with the ejection direction, not the angle
Draft only has meaning relative to the direction the part leaves the mold. Before any surface is reviewed, mark the intended draw direction on the CAD model and confirm it matches the parting-line strategy. If the enclosure has side actions, lifters or a split cavity, each moving section needs its own draw direction noted.
Use the draft analysis tool in the CAD or mold-flow software to color-code faces by their angle relative to that direction. The goal is not to hit a single number everywhere, but to see which faces are neutral, which are undercut, and which will drag against the tool. Cooling shrinkage can cause the part to grip the core, so faces that stay on the core side deserve particular attention.
Record the draw direction as a named view or annotation in the model so that the tooling buyer, molder and texture supplier all review the same orientation.
Map texture boundaries on the model
Texture is not a blanket finish. Mark on the CAD model exactly which faces receive texture, where the texture stops, and what happens at the boundary. A sharp texture edge on a drafted wall can create a visible line or a step if the boundary does not follow a natural parting line or a designed feature.
For each textured region, note whether the texture wraps over an edge, stops short of an edge, or fades out. Fade-outs and wrap-arounds are common sources of mismatch between the model and the physical sample, so they should be called out explicitly rather than left to the texture supplier's interpretation.
If a face is meant to remain smooth next to a textured face, mark that smooth zone as a separate surface finish requirement. The finish specification should reference the same face identifiers used in the CAD model.

| Review item | What to mark on the CAD model | What to state in the finish specification |
|---|---|---|
| Ejection direction | Named view or annotation showing the intended draw direction for each mold section | Reference to the draw direction view used for draft analysis |
| Texture boundaries | Faces and edges where texture starts, stops, fades or wraps | Description of each textured region using the same face identifiers |
| Cosmetic faces | Ranked list of faces that will be inspected cosmetically | Acceptance notes for each cosmetic face, including lighting conditions |
| Competing faces | Notes on where draft or texture requirements conflict between adjacent faces | Resolution agreed with the texture supplier |
| Sample observations | Photos or notes tied to specific faces and light direction | Reference sample or plaque used for comparison |
| Finish spec alignment | Face names and regions that match the finish spec | Cross-reference to the marked-up model view |
Identify competing cosmetic faces
Enclosures often have more than one face that will be judged by the customer. The A-surface may be the largest visible panel, but a textured grip area, a logo recess or a mating seam can also draw the eye. List every face that will be inspected cosmetically and rank them so that the mold maker knows where to prioritize polish, texture consistency and draft.
Competing cosmetic faces can pull the draft strategy in different directions. A deep texture on a side wall may require more draft to release cleanly, while an adjacent smooth face may need to stay within a tight flatness tolerance. Mark these conflicts on the model and resolve them with the texture supplier before the tool is cut.
Where two cosmetic faces meet at a corner, note how the texture and draft transition around that corner. A corner that looks acceptable in CAD can show a texture mismatch or a drag mark in the molded part.
Review sample observations against the model
When a sample or first-off part is available, compare it to the marked-up model under the same lighting conditions the customer will use. Low-angle light reveals texture depth, drag marks and surface waviness that are invisible under diffuse overhead light. Photograph the sample with the light direction noted so the observations can be tied back to specific faces.
Record observations by face: texture appearance, gloss variation, visible draft-related streaks, and any mismatch at texture boundaries. These notes become the basis for tool corrections and for the finish specification revision, rather than a general impression of the part.
If the sample was molded in a different material or texture depth than production, note that difference explicitly. Texture appearance and release behavior can change with material and surface depth, so a sample that passes in one configuration does not guarantee the same result in another.
Align the finish specification with the CAD markups
The finish specification should use the same face names, regions and boundaries as the CAD model. If the model marks a textured band on the side wall, the finish spec should describe that band in the same terms, including its start and stop lines and any fade or wrap behavior.
Avoid describing texture only by a supplier grade or a generic label. Add a reference to the marked-up model view and, where available, a physical texture plaque or sample that both parties have seen. This reduces the chance that the mold maker and texture supplier interpret the requirement differently.
Include a note on which faces are cosmetic, which are functional, and which are hidden. This helps the tooling buyer prioritize review effort and helps the molder understand where process variation is acceptable.
Confirm the handoff package before draft approval
Before approving the draft, confirm that the package includes the marked-up CAD model with draw direction, texture boundaries and cosmetic face rankings; the finish specification cross-referenced to the model; and any sample observations with lighting notes. Each item should be dated and attributed so that later changes can be traced.
Walk through the package with the mold maker and texture supplier together. The goal is a shared understanding of what will be built and how it will be judged, not a signed checklist. Any open question about draft, texture or cosmetic acceptance should be resolved or explicitly carried forward as a risk.
Keep the approved package as the baseline for tooling review. When the model or finish spec changes, update the markups and re-issue the package rather than relying on verbal agreements.
Common questions
Do I need a single draft angle for the whole textured enclosure?
No. Draft depends on the material, texture depth, part complexity and the depth of ejected features. The review should focus on whether each face has enough draft to release cleanly in the intended draw direction, not on a universal number.
How should texture boundaries be shown on the CAD model?
Mark the exact faces and edges where texture starts, stops, fades or wraps. Use the same face identifiers in the finish specification so the mold maker and texture supplier review the same regions.
What lighting should be used when reviewing a textured sample?
Use the same lighting conditions the customer will use, and include low-angle light to reveal texture depth, drag marks and surface waviness. Note the light direction with the observations so they can be tied back to specific faces.
Can a sample molded in one material guarantee the same texture result in another material?
No. Texture appearance and release behavior can change with material and surface depth. A sample that passes in one configuration should be treated as a reference, not a guarantee for a different material or texture depth.